Chrome ore crusher to reduce wear--Suifa Machinery

Chrome ore crusher to reduce wear -- Suifa Machinery

Method for reducing wear of chrome ore crusher -- Suifa Machinery, Gongyi Shifa Heavy Industry Machinery Manufacturing Co., Ltd.: 13073777338 , In the structure of the chromium ore crusher, the wear of the static and dynamic front plates often occurs, especially in the case of the lower 1/3 wear. Static and dynamic plate wear can cause the chrome ore crusher to fail to operate properly and lose its crushing capacity. The chromium ore crusher wears during the work process. This wear can be reduced and unavoidable. The wear will shorten the mechanical life, so it is reduced as much as possible. The chrome ore crushing machinery wears itself during processing of the ore. In order to minimize the loss of parts, one must adhere to the scientific choice of models ; the second is the rational use and selection. Once improperly selected, serious ones will cause long-term passive production of the factory, while lighter ones will also cause frequent consumption. Make post-selection conclusions.

The method of solving the galling of the chrome ore crusher is as follows: The newly installed jaw plate must be tightly fixed and installed, and the surface of the machine must be in contact with the machine smoothly. A layer of better plastic material can be placed between the jaw plate and the surface of the machine ; every batch of material entering the chrome ore crusher should be sampled. Once the material has undergone major changes, the chromium must be changed in time. The parameters of the mineral crusher are matched with the incoming materials ; the plate must be made of materials with high hardness, wear resistance and strong resistance ; the cement enterprise with the crushing production line of the mine can crush the coarse crushing of the mine and fine crushing of the cement. The same type of wear plate is used for interchange ; worn plates can be repaired by surfacing. In addition, during the work process, attention should be paid to the following: after the normal operation of the chromium ore crusher, the feed can be started ; the crushing materials should be added into the crushing chamber evenly, and side feeding or stacking should be avoided to prevent unilateral overload or overload ; Under normal circumstances, the temperature rise of the bearing does not exceed 35 °C , and the high temperature does not exceed 70 °C . If it exceeds 70 °C, the machine should be shut down immediately, and the cause must be eliminated . Before stopping the machine, the feeding operation shall be stopped first and the crushing chamber shall be After the crushed material is completely discharged, the motor can be turned off ; if the vehicle is stopped due to obstruction of the material in the crushing chamber, the motor should be immediately shut down and the material must be removed before restart . After the end of the tooth plate wears, the adjustable head can be adjusted. use.

For more help, please contact: Haofa Machinery Co., Ltd.

Wm related recommendation: chrome ore crusher chrome ore crusher chrome ore crusher price chrome ore crusher manufacturers

High Manganese Wear Parts

ZHEJIANG FULE MINING MACHINERY CO., LTD , https://www.flmachines.com